September 07, 2005

Flux This...

Note: All soldering fluxes are not the same...

Note: Use a tinning flux that contains silver...

Note: Failure to use good flux will result in massive headaches while pressure testing a system in the form of bad solder joints...

Note: Be thankful that 90% of the joints were done with the aforementioned tinning flux...

Note: There are a hell of a lot of joints here... 10% added up pretty fast...